“PVD coatings are processed at 550 celsius degrees and above. It the tool is objected to these degrees…”
Category - HEAT TREATMENT
“The biggest risk after heart treatment is distortion. The tool can be useless because of that.”
“It is very difficult to make forming and cutting tool without EDM operation.”
“Before PVD coatings such as chromium nitride, titanium nitride, titanium aluminium nitride, a fine nitriding layer should be done.”
COATINGS, FAILURE MECHANISMS, HEAT TREATMENT, TOOLS
Is nitriding applied on to forming and drawing tools?
“The goal nitriding on forming tools is to reduce the friction, prevent or reduce the…”
“The thick nitriding layer especially on 2379 can cause chipping.”
FAILURE MECHANISMS, HEAT TREATMENT, TOOL STEEL, TOOLS
Can 2379, Sverker 21 and Sleipner be nitrided?